Ice Crystallization During Cold-Start of a Proton-Exchange-Membrane Fuel Cell
Published Web Location
https://doi.org/10.1149/05801.0897ecstAbstract
Under subfreezing conditions, ice forms in the gas-diffusion (GDL) and catalyst layers (CL) of proton-exchange-membrane fuel cells (PEMFCs), drastically reducing cell performance. Although a number of strategies exist to prevent ice formation, there is little fundamental understanding of ice-crystallization mechanisms and kinetics within PEMFC components. We incorporate recently developed ice-crystallization kinetic expressions (1-3) within the CL and GDL of a simplified 1-D transient PEMFC cold-start model. To investigate the importance of ice-crystallization kinetics, we compare liquid-water and ice saturations, and cell-failure time predicted using our kinetic rate expression relative to that predicted using a thermodynamic-based approach. We identify conditions under which ice-crystallization kinetics is critical and elucidate the impact of freezing kinetics on low-temperature PEMFC operation. © The Electrochemical Society.
Many UC-authored scholarly publications are freely available on this site because of the UC's open access policies. Let us know how this access is important for you.
Main Content
Enter the password to open this PDF file:
-
-
-
-
-
-
-
-
-
-
-
-
-
-